(二)磨礦工藝 我國鐵礦磨礦工藝,大多數(shù)采用兩段磨礦流程,中小型選礦廠多采用一段磨礦流程。由于采用細篩再磨新工藝,近年來一些選礦廠已由兩段磨礦改為三段磨礦。采用的磨礦設備一般比較小,最大球磨機3.6m×6m,最大棒磨機3.2m×4.5m,最大自磨機5.5m×1.8m,礫磨機2.7m×3.6m。